Products
-
HASTELLOY B2 UNS N10665 W.NR.2.4617
Hastelloy B2 is a solid solution strengthened, nickel-molybdenum alloy, with significant resistance to reducing environments like hydrogen chloride gas, and sulfuric, acetic and phosphoric acids. Molybdenum is the primary alloying element which provides significant corrosion resistance to reducing environments. This nickel steel alloy can be used in the as-welded condition because it resists the formation of grain-boundary carbide precipitates in the weld heat-affected zone.
This nickel alloy provides excellent resistance to hydrochloric acid at all concentrations and temperatures. In additions, Hastelloy B2 has excellent resistance to pitting, stress corrosion cracking and to knife-line and heat-affected zone attack. Alloy B2 provides resistance to pure sulfuric acid and a number of non-oxidizing acids.
-
Hastelloy
High Temperature Alloy Chemical composition Grade C P S Mn Si Ni Cr Co Cu Fe N Mo Al W V Ti other no greater than HastelloyB 0.05 0.04 0.03 1 1 base ≤1 ≤2.5 - 4~6 - 26~30 - - 0.2~0.4 - - HastelloyB-2 0.02 0.04 0.03 1 0.1 base ≤1 ≤1 - ≤2 - 26~30 - - - - HastelloyB-3 0.01 0.04 0.03 3 0.1 ≥65 1~3 ≤3 ≤0.2 1~3 - 27~32 ≤0.5 ≤3 ≤0.2 ≤0.2 - ... -
ALLOY 718 MATERIAL DATA SHEETS
Inconel Alloy 718 A precipitation-hardenable nickel-chromium alloy also containing significant amounts of iron, niobium, and molybdenum along with lesser amounts of aluminum and titanium. It combines corrosion resistance and high strength with outstanding weldability including resistance to postweld cracking. The alloy has excellent creep-rupture strength at temperatures to 1300°F (700°C). Used in gas turbines, rocket motors, spacecraft, nuclear reactors, pumps, and tooling. INCONEL alloy 718SPF™ is a special version of INCONEL alloy 718, designed for superplastic forming.
UNS: N07718
W.Nr.: 2.4668
-
Monel 400 Uns N04400 W.Nr. 2.4360 And 2.4361
MONEL nickel-copper alloy 400 (UNS N04400) is a solid-solution alloy that can be hardened only by cold working. It has high strength and toughness over a wide temperature range and excellent resistance to many corrosive environments. Alloy 400 is widely used in many fields, especially marine and chemical processing. Typical applications are valves and pumps; pump and propeller shafts; marine fixtures and fasteners; electrical and electronic components; springs; chemical processing equipment; gasoline and fresh water tanks; crude petroleum stills, process vessels and piping; boiler feed water heaters and other heat exchangers; and deaerating heaters.Chemical Compositions
-
Nimonic
High Temperature Alloy Chemical composition Grade C Si Mn S P Cr Ni Fe Cu Ti Al Co other no greater than Nimonic90 0.13 1 1 0.015 18~21 base ≤1.5 ≤0.2 2~3 1~2 15~21 lead≤0.002 B≤0.02 Zr≤0.15 Nimonic91 0.1 1 1 0.015 27~30 base ≤1 ≤0.5 1.9~2.7 0.9~1.5 19~21 Nb0.4~1.1 B0.002~0.01 Zr≤0.1 Alloy property minimum Grade state tensile strength RmN/m㎡ Yield Strength Rp0.2N/... -
ALLOY 825 MATERIAL DATA SHEETS
Sandmeyer Steel Company stocks Alloy 825 nickel alloy plate in thicknesses from .1875″ (4.8mm) through 2.00″ (50.8mm) for corrosion resistant applications in the air pollution control, chemical and petrochemical, food processing, nuclear, offshore oil and gas production, ore processing, petroleum refining, steel pickling and waste disposal industries.
-
High Temperature Alloy
Application Chemistry Typical Carbon 0.080 max Manganese 2.00 max Silicon 0.75 max Chromium 24.00- 26.00 Nickel 19.00- 22.00 Molybdenum 0.75 max Phosphorus 0.040 max Physical Properties Density 0.29 lbs/in³ 9.01 g/cm³ Electrical Resistivity microhm-in (microhm-cm) 68°F (20°C) 37.0 (94.0) Specific Heat BTU/lb/°F (kJ/kg•K) 32-212°F (0-100°C) 0.12 (0.50) Thermal Conductivity BTU/hr/ft²/ft/°F (W/m•K) At 212°F (100°C) 8.... -
Nitronic
High Temperature Alloy Chemical composition Grade C Si Mn S P Cr Ni Fe Mo Ti Cu Nb N other no greater than Nitronic50 0.06 1 4~6 0.03 0.04 20.5~23.5 11.5~13.5 base 1.5~3 - - 0.1~0.3 0.2~0.4 - Nitronic60 0.1 3.5~4.5 7~9 0.03 0.04 16~18 8~9 base — — — — 0.08~0.18 - Alloy property minimum Grade state tensile strength RmN/m㎡ Yield Strength Rp0.2N/m㎡ Elongation As% B... -
17-4PH Material Data Sheet
International identifiers
AISI 630, ASTM A564-89 17-4PH, JIS SCS24 / SUS630, AFNOR Z7CNU15-05 / Z7CNU17-04
-
High Precision Alloy
High Temperature Alloy Chemical composition Grade C Si Mn S P Cr Ni Mo Cu Fe Al Co Ti no greater than 1J50 0.03 0.15~0.3 0.3~0.6 0.02 0.02 - 49.5~50.5 - ≤0.2 base — — — 1J79 0.03 0.3~0.5 0.6~1.1 0.02 0.02 - 78.5~80.5 3.8~4.1 ≤0.2 base — — — 3J53 0.05 0.8 0.8 0.02 0.02 5.2~5.8 41.5~43 0.7~0.9 — base 0.5~0.8 — 2.3~2.7 4J29 0.03 0.3 0.5 0.02 0.02 ... -
Nickel
High Temperature Alloy Chemical composition Grade Ni Fe Cu C Mn S Si Nickel200 99 ≤0.4 ≤0.25 ≤0.15 ≤0.35 ≤0.01 ≤0.35 Nickel201 99 ≤0.4 ≤0.25 ≤0.02 ≤0.35 ≤0.01 ≤0.35 Alloy property minimum product form condition tensile strength RmN/m㎡ Yield Strength Rp0.2N/m㎡ Elongation As% Brinell hardness HB stick and strip hot rolled 60~85 15~45 35~55 45~80 stick and strip cold drawn or annealed 55~75 15... -
Biphase Stainless Steel
High Temperature Alloy Chemical composition Grade C Si Mn S P Cr Ni Mo Cu N W other no greater than F51 0.03 1 2 0.02 0.03 21~23 4.5~6.5 2.5~3.5 - 0.08~0.2 - - F53 0.03 0.8 1.2 0.02 0.035 24~26 6~8 3~5 ≤0.5 0.24~0.32 — - F55 0.03 1 1 0.01 0.03 24~26 6~8 3~4 0.5~1 0.2~0.3 0.5~1 - 329 0.08 1 1.5 0.03 0.035 23~28 3~6 1~3 - - - - A4 ...